USA AMS SA-814/SA-814M , SA-813 TPXM-11 Specialsteel Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | SA-813 TPXM-11 | Austenite | AMS | USA | Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe |
C | Si | Mn | P | S | Cr | Ni | N |
---|---|---|---|---|---|---|---|
≤0.04 | ≤1.00 | 8.00 -10.0 | ≤0.06 | ≤0.03 | 19.0 -21.5 | 5.50 -7.50 | 0.15 -0.40 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
117 (≥) | 584 (≥) | 33 | 31 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
24 | - | - | 0.21 | - | |||
934 | 679 | - | 11.3 | 323 | - | ||
825 | - | 21 | 23.2 | 132 | 144 |
Heat treated : 1675°C - 1719°C
SA-814/SA-814M | Specification for Cold-Worked Welded Austenitic Stainless Steel Pipe | SA-814-SA-814M----.pdf |