USA SAE A 213/A 213M (2013), A 213 N08904 Specialsteel Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 213 N08904 | Austenite | SAE | USA | Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes |
C | Mn | Si | P | S | Cr | Ni | Mo | Cu |
---|---|---|---|---|---|---|---|---|
≤0.02 | ≤2.00 | ≤1.00 | ≤0.045 | ≤0.035 | 19.00 -23.00 | 23.00 -28.00 | 4.00 -5.00 | 1.00 -2.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
427 (≥) | 392 (≥) | 31 | 22 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
11 | - | - | 0.32 | - | |||
731 | 928 | - | 14.3 | 432 | - | ||
431 | - | 21 | 44.2 | 133 | 124 |
Heat treated : 1682°C - 1854°C
Grade | Standard | Country | Application |
---|---|---|---|
904L | |||
INCO alloy 904L | |||
904L | |||
904L(N08904) | |||
N08904 | |||
N08904 | |||
N08904 | |||
UNS N08904 |
A 213/A 213M (2013) | Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes | A-213-A-213M-(2013).pdf |