USA SAE A 965/A 965M (2012) , A 965 Grade FXM11 Specialsteel Steel Forgings, Austenitic, for Pressure and High Temperature Parts and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 965 Grade FXM11 | Austenite | SAE | USA | Steel Forgings, Austenitic, for Pressure and High Temperature Parts |
C | Si | Mn | P | S | Cr | Ni | N |
---|---|---|---|---|---|---|---|
≤0.04 | ≤1.00 | 8.00 -10.0 | ≤0.06 | ≤0.03 | 19.0 -21.5 | 5.50 -7.50 | 0.15 -0.40 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
634 (≥) | 729 (≥) | 43 | 42 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 311 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.24 | - | |||
952 | 767 | - | 12.3 | 443 | - | ||
743 | - | 33 | 11.2 | 442 | 441 |
Heat treated : 1436°C - 1865°C
A 965/A 965M (2012) | Steel Forgings, Austenitic, for Pressure and High Temperature Parts | A-965-A-965M--(2012)-.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...