USA SAE A 269 (2010), A 269 S21904 Specialsteel Seamless and Welded Austenitic Stainless Steel Tubing for General Service and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 269 S21904 | Austenite | SAE | USA | Seamless and Welded Austenitic Stainless Steel Tubing for General Service |
C | Mn | Si | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.04 | 8.00 -10.00 | ≤1.00 | ≤0.06 | ≤0.03 | 19.00 -21.50 | 5.50 -7.50 | ≤ ≥ | 0.15 -0.40 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
965 (≥) | 473 (≥) | 22 | 23 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
44 | - | - | 0.32 | - | |||
171 | 222 | - | 44.3 | 342 | - | ||
848 | - | 43 | 43.2 | 134 | 223 |
Heat treated : 1864°C - 1682°C
A 269 (2010) | Seamless and Welded Austenitic Stainless Steel Tubing for General Service | A-269-(2010).pdf |