USA AISI S50200 Specialsteel Chromium Heat Resisting Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | S50200 | Martensite | AISI | USA | Chromium Heat Resisting Steel |
C | Mn | Si | P | S | Cr | Ni | Mo |
---|---|---|---|---|---|---|---|
≤0.10 | ≤1.00 | ≤1.00 | ≤0.04 | ≤0.03 | 4.00 -6.00 | ≤ ≥ | 0.40 -0.65 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
926 (≥) | 311 (≥) | 22 | 22 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.22 | - | |||
864 | 244 | - | 11.3 | 441 | - | ||
211 | - | 23 | 23.2 | 124 | 223 |
Heat treated : 1746°C - 1387°C
Grade | Standard | Country | Application |
---|---|---|---|
1.5028 | |||
1.5022 | |||
1.5023 | |||
1.5024 | |||
1.5025 | |||
1.5026 | |||
1.5026 | |||
1.5029 | |||
1.4502 | |||
1.4502 | |||
MONEL alloy 502 | |||
UNS T31502 | |||
UNS J02502 | |||
UNS W50205 | |||
UNS W50206 | |||
UNS W50208 | |||
UNS W50218 | |||
UNS W50215 | |||
UNS W50216 | |||
AWS E502 |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com