USA SAE ASTM 205 Specialsteel Stainless steel and heat resistant steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | ASTM 205 | Austenite | SAE | USA | Stainless steel and heat resistant steel |
C | Si | Mn | P | S | Cr | Ni | N |
---|---|---|---|---|---|---|---|
0.12 -0.25 | ≤1.00 | 14.0 -15.5 | ≤0.06 | ≤0.03 | 16.5 -18.0 | 1.00 -1.75 | 0.32 -0.40 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
254 (≥) | 767 (≥) | 42 | 12 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.33 | - | |||
282 | 931 | - | 34.3 | 131 | - | ||
753 | - | 23 | 42.2 | 343 | 311 |
Heat treated : 1311°C - 1473°C
Grade | Standard | Country | Application |
---|---|---|---|
AISI 205 Stainless Steel | |||
1.2056 | |||
1.2057 | |||
205 | |||
S20500 | |||
S32050 | |||
S32053 | |||
2205 | |||
S32205 | |||
2205(C) | |||
HASTELLOY alloy D-205 | |||
Nickel 205 | |||
SM 2050 | |||
S32050 | |||
S32053 | |||
S32205 | |||
2205 | |||
S32050 | |||
S32050 | |||
S32050 |