USA SAE A 554 (2011), A 554 S44400 Specialsteel Welded Stainless Steel Mechanical Tubing and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 554 S44400 | Ferrite | SAE | USA | Welded Stainless Steel Mechanical Tubing |
C | Mn | Si | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.025 | ≤1.00 | ≤1.00 | ≤0.04 | ≤0.03 | 17.50 -19.50 | ≤1.00 | 1.75 -2.50 | ≤0.035 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
345 (≥) | 772 (≥) | 11 | 24 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
22 | - | - | 0.43 | - | |||
825 | 422 | - | 12.3 | 132 | - | ||
475 | - | 24 | 42.2 | 313 | 242 |
Heat treated : 1857°C - 1721°C
Grade | Standard | Country | Application |
---|---|---|---|
1.4449 | |||
1.4446 | |||
1.4448 | |||
1.4440 | |||
1.4440 | |||
444 | |||
S44400 | |||
444 | |||
S44450 | |||
TP44400 | |||
S44400 | |||
TP44400 | |||
S44400 | |||
S44400 | |||
S44400 | |||
AMS 6444G | |||
SUS444 | |||
SUS444 | |||
SUS444 | |||
SUS444TP |
A 554 (2011) | Welded Stainless Steel Mechanical Tubing | A-554-(2011).pdf |