USA AISI S63198 Specialsteel Iron Base Superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | S63198 | Austenite | AISI | USA | Iron Base Superalloy |
C | Mn | Si | P | S | Cr | Ni | Mo |
---|---|---|---|---|---|---|---|
0.28 -0.35 | 0.75 -1.50 | 0.30 -0.80 | ≤0.04 | ≤0.03 | 18.00 -21.00 | 8.00 -11.00 | 1.00 -1.75 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
395 (≥) | 983 (≥) | 44 | 13 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.11 | - | |||
555 | 424 | - | 14.3 | 443 | - | ||
487 | - | 22 | 42.2 | 434 | 311 |
Heat treated : 1549°C - 1381°C
Grade | Standard | Country | Application |
---|---|---|---|
1.6513 | |||
1.6511 | |||
1.6513 | |||
1.6512 | |||
1.6512 | |||
1.6515 | |||
1.6515 | |||
S31651 | |||
651 | |||
651 | |||
S31651 | |||
S31651 | |||
S31651 | |||
S31651 | |||
S31651 | |||
AMS 6512B | |||
UNS J94651 | |||
UNS J94651 | |||
651 | |||
316N(S31651) |