USA SAE A 580/A 580M (2012), A 580 S34700 Specialsteel Stainless Steel Wire and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 580 S34700 | Austenite | SAE | USA | Stainless Steel Wire |
C | Mn | Si | P | S | Cr | Ni | Ta |
---|---|---|---|---|---|---|---|
≤0.08 | ≤2.00 | ≤1.00 | ≤0.045 | ≤0.03 | 17.00 -19.00 | 9.00 -13.00 | ≤1.10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
725 (≥) | 413 (≥) | 23 | 32 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 121 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
24 | - | - | 0.21 | - | |||
189 | 262 | - | 11.3 | 133 | - | ||
533 | - | 23 | 22.2 | 141 | 114 |
Heat treated : 1695°C - 1742°C
Grade | Standard | Country | Application |
---|---|---|---|
1.4347 | |||
347 | |||
S34700 | |||
347H | |||
S34709 | |||
S34751 | |||
347LN | |||
S34700 | |||
347 | |||
S34709 | |||
347H | |||
TP347 | |||
S34700 | |||
TP347H | |||
S34709 | |||
TP347HFG | |||
S34710 | |||
TP347LN | |||
S34751 | |||
TP347 |