USA AISI N08330 Specialsteel Ni-Fe-Cr Alloy Solid Solution Strengthened and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | N08330 | Austenite | AISI | USA | Ni-Fe-Cr Alloy Solid Solution Strengthened |
C | Mn | Si | P | S | Cr | Ni |
---|---|---|---|---|---|---|
≤0.15 | ≤2.00 | ≤1.50 | ≤0.045 | ≤0.04 | 14.00 -17.00 | 33.00 -37.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
145 (≥) | 437 (≥) | 22 | 23 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.31 | - | |||
131 | 565 | - | 32.3 | 342 | - | ||
888 | - | 31 | 14.2 | 244 | 244 |
Heat treated : 1317°C - 1693°C
Grade | Standard | Country | Application |
---|---|---|---|
AISI 1330 | |||
UNS G23300 | |||
AISI 1330 | |||
1.3302 | |||
G-X330NiCr4-2 | |||
RA 330 | |||
RA 330 Mod. | |||
RA 330 TX | |||
RA 330-04 | |||
MT-330 | |||
A2330 | |||
2330 | |||
ASTM 1330 | |||
UNS G13300 | |||
ASTM 1330H | |||
UNS H13300 | |||
UNS G10330 | |||
SAE 1330H | |||
UNS H13300 | |||
AMS 6330D |