USA AISI S32100 Specialsteel Austenitic Chromium Nickel Titanium Stainless Steel (Titanium Stabilized) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | S32100 | Austenite | AISI | USA | Austenitic Chromium Nickel Titanium Stainless Steel (Titanium Stabilized) |
C | Mn | Si | P | S | Cr | Ni | N |
---|---|---|---|---|---|---|---|
≤0.08 | ≤2.00 | ≤1.00 | ≤0.045 | ≤0.03 | 17.00 -19.00 | 9.00 -12.00 | ≤0.10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
913 (≥) | 248 (≥) | 44 | 43 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.41 | - | |||
165 | 486 | - | 41.3 | 232 | - | ||
614 | - | 42 | 21.2 | 411 | 334 |
Heat treated : 1533°C - 1974°C
Grade | Standard | Country | Application |
---|---|---|---|
1.7321 | |||
321 | |||
S32100 | |||
321H | |||
S32109 | |||
S32101 | |||
S32100 | |||
321 | |||
S32109 | |||
321 H | |||
S32101 | |||
TP321 | |||
S32100 | |||
TP321H | |||
S32109 | |||
TP321 | |||
S32100 | |||
TP321H | |||
S32109 | |||
TP321 |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com