USA SAE A 814/A 814M (2008), A814 S32100 Specialsteel Cold-Worked Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A814 S32100 | Austenite | SAE | USA | Cold-Worked Welded Austenitic Stainless Steel Pipe |
C | Mn | Si | P | S | Cr | Ni | N |
---|---|---|---|---|---|---|---|
≤0.08 | ≤2.00 | ≤1.00 | ≤0.045 | ≤0.03 | 17.00 -19.00 | 9.00 -12.00 | ≤0.10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
514 (≥) | 496 (≥) | 23 | 32 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.22 | - | |||
781 | 477 | - | 33.3 | 333 | - | ||
293 | - | 42 | 44.2 | 144 | 434 |
Heat treated : 1436°C - 1848°C
Grade | Standard | Country | Application |
---|---|---|---|
1.7321 | |||
321 | |||
S32100 | |||
321H | |||
S32109 | |||
S32101 | |||
S32100 | |||
321 | |||
S32109 | |||
321 H | |||
S32101 | |||
TP321 | |||
S32100 | |||
TP321H | |||
S32109 | |||
TP321 | |||
S32100 | |||
TP321H | |||
S32109 | |||
TP321 |
A 814/A 814M (2008) | Cold-Worked Welded Austenitic Stainless Steel Pipe | A-814-A-814M-(2008).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com