USA AISI S31703 Specialsteel Austenitic Chromium Nickel Molybdenum Stainless Steel (Low Carbon) (317L) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | S31703 | Austenite | AISI | USA | Austenitic Chromium Nickel Molybdenum Stainless Steel (Low Carbon) (317L) |
C | Mn | Si | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.03 | ≤2.00 | ≤1.00 | ≤0.045 | ≤0.03 | 18.00 -20.00 | 11.00 -15.00 | 3.00 -4.00 | ≤0.10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
798 (≥) | 825 (≥) | 33 | 43 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 121 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.42 | - | |||
423 | 339 | - | 41.3 | 312 | - | ||
712 | - | 12 | 32.2 | 141 | 321 |
Heat treated : 1486°C - 1311°C
Grade | Standard | Country | Application |
---|---|---|---|
317L | |||
317LM | |||
317LMN | |||
317LN | |||
317LM | |||
317L4 | |||
317L | |||
317LM | |||
317LMN | |||
317LN | |||
TP317L | |||
TP317LM | |||
TP317LMN | |||
TP317L | |||
TP317L | |||
AWS E317L | |||
AWS ER317L | |||
SUS317L | |||
SUS317LN | |||
SUS317LFB |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com