USA SAE A 813/A 813M (2009), A 813 S31653 Specialsteel Single- or Double-Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 813 S31653 | Austenite | SAE | USA | Single- or Double-Welded Austenitic Stainless Steel Pipe |
C | Si | Mn | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.03 | ≤0.75 | ≤2.00 | ≤0.045 | ≤0.035 | 16.0 -18.0 | 10.0 -14.0 | 2.00 -3.00 | 0.10 -0.16 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
388 (≥) | 648 (≥) | 24 | 22 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 413 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.34 | - | |||
397 | 161 | - | 34.3 | 314 | - | ||
593 | - | 14 | 23.2 | 113 | 311 |
Heat treated : 1359°C - 1462°C
Grade | Standard | Country | Application |
---|---|---|---|
316LN | |||
316LN | |||
TP316LN | |||
TP316LN | |||
TP316LN | |||
TP316LN | |||
TP316LN | |||
SUS316LN | |||
SUS316LN | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 |
A 813/A 813M (2009) | Single- or Double-Welded Austenitic Stainless Steel Pipe | A-813-A-813M-(2009).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com