C | Si | Mn | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.03 | ≤0.75 | ≤2.00 | ≤0.045 | ≤0.035 | 16.0 -18.0 | 10.0 -14.0 | 2.00 -3.00 | 0.10 -0.16 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
729 (≥) | 971 (≥) | 33 | 32 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.11 | - | |||
718 | 734 | - | 32.3 | 444 | - | ||
837 | - | 11 | 21.2 | 324 | 311 |
Heat treated : 1991°C - 1367°C
Grade | Standard | Country | Application |
---|---|---|---|
316LN | |||
316LN | |||
TP316LN | |||
TP316LN | |||
TP316LN | |||
TP316LN | |||
TP316LN | |||
SUS316LN | |||
SUS316LN | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 | |||
S31653 |
A 943/A 943M (2009) | Spray-Formed Seamless Austenitic Stainless Steel Pipes | A-943-A-943M-(2009)-.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com