SKC3 Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel | SKC3 | |||
| SK75M | |||||
| SK6M | |||||
| SK65M | |||||
| SK7M | |||||
| SKS2M | |||||
| SKS5M | |||||
| SKS7M | |||||
| SKS51M | |||||
| SKS81M | |||||
| SKS95M | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.7-0.85 | 0.15-0.35 | 0.5 | 0.03 | 0.03 | ≤0.2 | ≤0.25 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| ≤0.25 | ≤0.25 | ≤0.25 | ||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 644 (≥) | 348 (≥) | 21 | 11 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 32 | - | - | 0.21 | - | |||
| 132 | 594 | - | 34.3 | 444 | - | ||
| 982 | - | 44 | 21.2 | 231 | 334 | 
Heat treated : 1267°C - 1452°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| SKC3 | JIS | Japan | Hollow Steel | 
| SKC31 | JIS | Japan | Hollow Steel | 
| SKC31① | China | Carbide for cutting tools | |
| SKC31① | China | Carbide for cutting tools | |
| SKC31① | China | Carbide for cutting tools | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com