1.2365 Tool Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Tool Steel | 1.2365 | |||
| X38CrMoV5-1 |
|||||
| X37CrMoV5-1 |
|||||
| 1.2344 |
|||||
| X40CrMoV5-1 |
|||||
| 1.2345 |
|||||
| X50CrMoV5-1 |
|||||
| 1.2357 |
|||||
| 50CrMoV13-14 |
|||||
| 1.2360 |
|||||
| X48CrMoV8-1-1 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| 0.28-0.35 | 0.10-0.40 | 0.15-0.45 | 0.030 | 0.020 | 2.70-3.20 | 2.50-3.00 | V 0.40-0.70 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 646 (≥) | 524 (≥) | 24 | 21 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 32 | - | - | 0.42 | - | |||
| 632 | 922 | - | 22.3 | 142 | - | ||
| 727 | - | 11 | 34.2 | 314 | 421 |
Heat treated : 1943°C - 1125°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...