Japan JIS Z10 ultra-particulate carbide and Z10 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | Z10 | JIS | Japan | ultra-particulate carbide |
E1 |
|||||
E2 |
|||||
E2 |
|||||
E3 |
|||||
E3 |
|||||
E4 |
|||||
E5 |
|||||
Z01 |
|||||
Z01 |
|||||
Z10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
622 (≥) | 166 (≥) | 12 | 22 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.43 | - | |||
378 | 163 | - | 21.3 | 234 | - | ||
229 | - | 11 | 23.2 | 244 | 314 |
Heat treated : 1777°C - 1713°C
Grade | Standard | Country | Application |
---|---|---|---|
Z10 | JIS | Japan | ultra-particulate carbide |
Z10 | JIS | Japan | ultra-particulate carbide |
Z10CNDA15-07 | AFNOR | France | Stainless Steel Plate & Steel Strip |
Z10NC32-21 | AFNOR | France | Stainless Steel Plate & Steel Strip |
Z10C3 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) |
Z100CD17CI | AFNOR | France | Cutlery stainless steel |
Z10CNWT17-13B | AFNOR | France | Heat-Resistant Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com