France AFNOR TH1 Carbide for cutting tools and TH1 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | TH1 | AFNOR | France | Carbide for cutting tools |
TG4 |
|||||
TG4 |
|||||
TG4 |
|||||
TG5 |
|||||
TG5 |
|||||
TG6 |
|||||
TG6 |
|||||
TH1 |
|||||
TH1 |
|||||
TH1 |
Co(%) |
---|
5.6 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
862 (≥) | 449 (≥) | 22 | 13 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.12 | - | |||
147 | 889 | - | 11.3 | 342 | - | ||
744 | - | 42 | 24.2 | 314 | 342 |
Heat treated : 1256°C - 1742°C
Grade | Standard | Country | Application |
---|---|---|---|
TH1 | AFNOR | France | Carbide for cutting tools |
TH1 | AFNOR | France | Carbide for cutting tools |
TH1 | AFNOR | France | Carbide for cutting tools |
TH1 | AFNOR | France | Carbide for cutting tools |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...