X39CrMo17-1 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | X39CrMo17-1 | |||
| X14CrMoS17 |
|||||
| X6CrMo17 |
|||||
| X70CrMo15 |
|||||
| X55CrMo14 |
|||||
| X110CrMoV15 |
|||||
| X90CrMoV18 |
|||||
| X6CrMo17-1 |
|||||
| X50CrMoV15 |
|||||
| X38CrMoV15 |
|||||
| X20CrMo13 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| 0.33-0.45 | 1.00 | 1.00 | 0.040 | 0.015 | 15.5-17.5 | ≤1.00 | 0.80-1.30 |
.
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 564 (≥) | 612 (≥) | 22 | 12 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.12 | - | |||
| 769 | 768 | - | 31.3 | 211 | - | ||
| 259 | - | 23 | 42.2 | 331 | 114 |
Heat treated : 1685°C - 1198°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| EN X39CrMo17-1 | EN | Euronorm Stainless Steel | |
| EN X39CrMo17-1 | EN | Euronorm Stainless Steel | |
| EN X39CrMo17-1 | EN | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com