201L Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | 201L | |||
| 1.4875 | |||||
| 1.4881 | |||||
| 1.4882 | |||||
| 2.4955 | |||||
| 1.5028 | |||||
| 1.5122 | |||||
| 16-8-2H | |||||
| S16800 | |||||
| 201 | |||||
| S20100 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.03 | 0.75 | 5.50-7.50 | 0.045 | 0.030 | 16.0-18.0 | 3.50-5.50 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| N | Co | Pb | B | Other | ||
| ≤0.25 | ||||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 111 (≥) | 938 (≥) | 34 | 32 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.43 | - | |||
| 475 | 735 | - | 33.3 | 331 | - | ||
| 669 | - | 42 | 13.2 | 111 | 411 | 
Heat treated : 1574°C - 1993°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com