1.4318 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | 1.4318 | |||
| 1.4120 |
|||||
| 1.4122 |
|||||
| 1.4125 |
|||||
| 1.4301 |
|||||
| 1.4303 |
|||||
| 1.4305 |
|||||
| 1.4306 |
|||||
| 1.4310 |
|||||
| 1.4311 |
|||||
| 1.4313 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| ≤0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 16.5-18.5 | 6.00-8.00 | -------- | N 0.10-0.20 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 436 (≥) | 263 (≥) | 41 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.22 | - | |||
| 463 | 425 | - | 24.3 | 132 | - | ||
| 517 | - | 12 | 41.2 | 113 | 342 |
Heat treated : 1126°C - 1352°C