France AFNOR Z9CNDA15-07 Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) and Z9CNDA15-07 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | Z9CNDA15-07 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) |
Z3CN19-11 |
|||||
Z3CND18-12-02 |
|||||
Z3CNU18-10 |
|||||
Z3CNU23-04Az |
|||||
Z3NCDU28-20 |
|||||
Z4CND22-16-03Az |
|||||
Z4CNDAT13-09 |
|||||
Z5CND27-05Az |
|||||
Z5CNDU22-07 |
|||||
Z6NCTDV25-15B |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Al(%) |
---|---|---|---|---|---|---|---|---|
Max 0.09 | Max 0.75 | Max 1.00 | Max 0.040 | Max 0.025 | 14.0-16.0 | 6.50-7.50 | 2.00-3.00 | 0.75-1.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
487 (≥) | 924 (≥) | 33 | 41 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.31 | - | |||
975 | 871 | - | 42.3 | 233 | - | ||
418 | - | 41 | 12.2 | 221 | 121 |
Heat treated : 1579°C - 1488°C
Grade | Standard | Country | Application |
---|---|---|---|
Z9CNDA15-07 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com