Z3CN19-11FF Cold drawn stainless steel bar and wire rod(NF A 35-577(1990)) and Z3CN19-11FF Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | Z3CN19-11FF | Cold drawn stainless steel bar and wire rod(NF A 35-577(1990)) | ||
Z5CND27-05Az |
|||||
Z5CNDU22-07 |
|||||
Z6NCTDV25-15B |
|||||
Z9CNDA15-07 |
|||||
Z10C3 |
|||||
Z11CF13 |
|||||
Z12CND16-05-03 |
|||||
Z13CF17 |
|||||
Z15CN16-02 |
|||||
Z29CF13 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) |
---|---|---|---|---|---|---|
Max 0.03 | 0.30-0.60 | 0.30-1.00 | Max 0.040 | Max 0.010 | 18.0-19.0 | 10.0-11.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
293 (≥) | 121 (≥) | 13 | 21 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.44 | - | |||
158 | 272 | - | 32.3 | 244 | - | ||
646 | - | 44 | 43.2 | 321 | 111 |
Heat treated : 1983°C - 1983°C
Grade | Standard | Country | Application |
---|---|---|---|
Z3CN19-11FF | Cold drawn stainless steel bar and wire rod(NF A 35-577(1990)) |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com