GX4CrNiMo16-5-1 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Mould Steel | GX4CrNiMo16-5-1 | |||
G35NiCrMo6-6 |
|||||
1.6579 |
|||||
G42CrMo |
|||||
1.7231 |
|||||
GX3CrNi13-4 |
|||||
1.6982 |
|||||
GX4CrNi13-4 |
|||||
1.4317 |
|||||
GX4CrNi16-4 |
|||||
1.4421 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.06 | 0.80 | 1.00 | 0.035 | 0.025 | 15.0-17.0 | 4.00-6.00 |
Mo | Al | Cu | Nb | Ti | V | Ce |
0.70-1.50 | ||||||
N | Co | Pb | B | Other | ||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
817 (≥) | 773 (≥) | 22 | 31 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.12 | - | |||
753 | 628 | - | 14.3 | 134 | - | ||
363 | - | 44 | 14.2 | 122 | 444 |
Heat treated : 1125°C - 1642°C
Grade | Standard | Country | Application |
---|---|---|---|
GX4CrNiMo16-5-1 | Spain structural alloy steel | ||
EN GX4CrNiMo16-5-1 | EN | Euronorm Structural steel | |
EN GX4CrNiMo16-5-1 | EN | Euronorm Stainless Steel |