C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.20-0.26 | 0.40 | 0.50-0.80 | 0.030 | 0.020 | 11.3-12.2 | ≤ 1.00 |
Mo | Al | Cu | Nb | Ti | V | Ce |
1.00-1.20 | 0.25-0.35 | |||||
N | Co | Pb | B | Other | ||
W≤0.50 | ||||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
844 (≥) | 484 (≥) | 43 | 32 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.24 | - | |||
779 | 727 | - | 12.3 | 314 | - | ||
899 | - | 42 | 43.2 | 433 | 343 |
Heat treated : 1558°C - 1718°C
Grade | Standard | Country | Application |
---|---|---|---|
GX23CrMoV12-1 | Spain structural alloy steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com