G20Mo5 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Mould Steel | G20Mo5 | |||
| G-X120Mn12 |
|||||
| 1.3401 |
|||||
| G-X110Mn14 |
|||||
| 1.3402 |
|||||
| GP240GH |
|||||
| 1.0619 |
|||||
| GP240GR |
|||||
| 1.0621 |
|||||
| GP280GH |
|||||
| 1.0625 |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.15-0.23 | 0.60 | 0.50-1.00 | 0.025 | 0.020 | ||
| Mo | Al | Cu | Nb | Ti | V | Ce |
| 0.40-0.60 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 738 (≥) | 587 (≥) | 44 | 42 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.14 | - | |||
| 561 | 385 | - | 23.3 | 433 | - | ||
| 949 | - | 34 | 12.2 | 311 | 141 |
Heat treated : 1785°C - 1613°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| G20Mo5 | Spain structural alloy steel | ||
| EN G20Mo5 | EN | Euronorm Structural steel |