1.4573 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Mould Steel | 1.4573 | |||
1.4525 |
|||||
GX2CrNiMoCuN20-18 |
|||||
1.4531 |
|||||
GX2CrNiMoCuN25-20 |
|||||
1.4536 |
|||||
GX1CrNiMoCuN25-20-5 |
|||||
1.4538 |
|||||
GX2CrNiMnMoNNb21-15-4-3 |
|||||
1.4569 |
|||||
GX3CrNiMoCuN24-6-5 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.04 | 1.00 | 1.00 | 0.030 | 0.020 | 22.0-25.0 | 4.50-6.50 |
Mo | Al | Cu | Nb | Ti | V | Ce |
4.50-6.00 | 1.50-2.50 | |||||
N | Co | Pb | B | Other | ||
0.15-0.25 | ||||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
333 (≥) | 667 (≥) | 23 | 24 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.43 | - | |||
332 | 669 | - | 21.3 | 244 | - | ||
656 | - | 32 | 41.2 | 144 | 342 |
Heat treated : 1841°C - 1222°C
Grade | Standard | Country | Application |
---|---|---|---|
W-Nr 1.4573 | DIN | Germany | Stainless steel |
W-Nr 1.4573 | DIN | Germany | Stainless steel |