1.4437 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Mould Steel | 1.4437 | |||
1.4340 |
|||||
GX6CrNiN26-7 |
|||||
1.4347 |
|||||
GX4CrNiM016-5-1 |
|||||
1.4405 |
|||||
GX2CrNiM0N19-11-2 |
|||||
1.4409 |
|||||
GX2CrNiMoN25-7-3 |
|||||
1.4417 |
|||||
GX6CrNiMo18-12 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.07 | 2.00 | 2.00 | 0.045 | 0.030 | 16.5-18.5 | 11.5-13.5 |
Mo | Al | Cu | Nb | Ti | V | Ce |
2.50-3.00 | ||||||
N | Co | Pb | B | Other | ||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
794 (≥) | 244 (≥) | 43 | 21 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.14 | - | |||
221 | 773 | - | 23.3 | 234 | - | ||
857 | - | 32 | 42.2 | 124 | 432 |
Heat treated : 1645°C - 1613°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...