IN-713 High Alloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | High Alloy | IN-713 | |||
HS-95 |
|||||
HS-188 |
|||||
HS-556 |
|||||
HTX |
|||||
HY 220 |
|||||
IN-100 |
|||||
IN-102 |
|||||
IN-162 |
|||||
IN-587 |
|||||
IN-597 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.08-0.2 | 0.5 | 0.25 | 12-14 | ... | ||
Mo | Al | Cu | Nb | Ti | V | Ce |
3.8-5.2 | 5.5-6.5 | 1.8-2.8 | 0.5-1.0 | |||
N | Co | Pb | B | Other | ||
0.005-0.015 |
Zr0.05-0.15 Fe≤2.50 |
|||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
356 (≥) | 913 (≥) | 33 | 32 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.43 | - | |||
153 | 292 | - | 14.3 | 242 | - | ||
356 | - | 34 | 14.2 | 133 | 123 |
Heat treated : 1188°C - 1539°C