France AFNOR Z6CNT18-10B Heat-Resistant Steel and Z6CNT18-10B Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Heat-Resistant Steel | Z6CNT18-10B | AFNOR | France | Heat-Resistant Steel |
| Z6CNDT17-13B |
|||||
| Z3CAT18 |
|||||
| Z5NCTDV26-15B |
|||||
| Z6CND17-13B |
|||||
| Z6CNNb18-12B |
|||||
| CNS NCF751 |
|||||
| CNS NCF800 |
|||||
| CNS NCF800H |
|||||
| CNS NCF825 |
|||||
| CNS NCF80A |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | B(%) | Ti(%) |
|---|---|---|---|---|---|---|---|---|
| 0.04-0.08 | Max 0.75 | Max 2.00 | Max 0.040 | Max 0.015 | 17.5-19.0 | 9.00-11.0 | 0.0015-0.0060 | 4(C+N) Max 0.60 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 325 (≥) | 376 (≥) | 13 | 13 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 112 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 32 | - | - | 0.13 | - | |||
| 815 | 585 | - | 22.3 | 213 | - | ||
| 324 | - | 42 | 33.2 | 121 | 122 |
Heat treated : 1221°C - 1342°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| Z6CNT18-10B | AFNOR | France | Heat-Resistant Steel |