20X20H14C2 Austenitic - Martensitic steel and 20X20H14C2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Heat-Resistant Steel | 20X20H14C2 | Austenitic - Martensitic steel | ||
| 08X17T | |||||
| 15X18Ю | |||||
| 15X25T | |||||
| 15X28 | |||||
| 20X13H4Γ9 | |||||
| 09X15H8Ю | |||||
| 07X16H6 | |||||
| 09X17H7Ю | |||||
| 08X17H5M3 | |||||
| 08X20H14C2 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|---|---|
| Max 0.20 | 2.00-3.00 | Max 1.50 | Max 0.035 | Max 0.025 | 19.0-22.0 | 12.0-15.0 | Max 0.30 | Max 0.20 | Max 0.20 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 828 (≥) | 459 (≥) | 43 | 41 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.33 | - | |||
| 887 | 762 | - | 42.3 | 331 | - | ||
| 964 | - | 13 | 44.2 | 141 | 342 | 
Heat treated : 1926°C - 1257°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| 20X20H14C2 | Austenitic - Martensitic steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com