SWRCH20K Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | SWRCH20K | |||
| SWRCH19A |
|||||
| SWRCH20A |
|||||
| SWRCH22A |
|||||
| SWRCH25A |
|||||
| SWRCH10K |
|||||
| SWRCH12K |
|||||
| SWRCH15K |
|||||
| SWRCH16K |
|||||
| SWRCH17K |
|||||
| SWRCH18K |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.18-0.23 | 0.1-0.35 | 0.3-0.6 | 0.03 | 0.035 | ≤0.2 | ≤0.2 |
| Mo | Al | Cu | Nb | Ti | V | Ce |
| ≤0.3 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 111 (≥) | 981 (≥) | 24 | 11 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.42 | - | |||
| 382 | 776 | - | 42.3 | 124 | - | ||
| 651 | - | 12 | 34.2 | 124 | 233 |