SEV245 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.19 | 0.15-0.6 | 0.8-1.6 | 0.03 | 0.03 | ||
Mo | Al | Cu | Nb | Ti | V | Ce |
0.1-0.4 | ≤ 0.7 | ≤0.05 | ≤0.19 | |||
N | Co | Pb | B | Other | ||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
922 (≥) | 463 (≥) | 33 | 11 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.12 | - | |||
315 | 282 | - | 23.3 | 312 | - | ||
378 | - | 34 | 22.2 | 431 | 224 |