S275MLH Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Carbon Steel | S275MLH | |||
S420NH |
|||||
1.8750 |
|||||
S420NLH |
|||||
1.8751 |
|||||
S460NH |
|||||
1.8953 |
|||||
S460NLH |
|||||
1.8956 |
|||||
S275MH |
|||||
1.8843 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.13 | 0.50 | 1.50 | 0.030 | 0.025 | ≤0.30 | |
Mo | Al | Cu | Nb | Ti | V | Ce |
≤0.20 | ≥ | 0.020≤0.050 | ≤ 0.050 | ≤ 0.08 | ||
N | Co | Pb | B | Other | ||
≤ 0.020 | ||||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
541 (≥) | 475 (≥) | 11 | 13 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 111 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.42 | - | |||
133 | 369 | - | 21.3 | 111 | - | ||
928 | - | 31 | 33.2 | 134 | 232 |
Heat treated : 1372°C - 1426°C
Grade | Standard | Country | Application |
---|---|---|---|
EN S275MLH | EN | Euronorm Structural steel |