P275NL2 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Carbon Steel | P275NL2 | |||
1.0490 |
|||||
S275N |
|||||
1.0491 |
|||||
S275NL |
|||||
1.0487 |
|||||
P275NH |
|||||
WStE 285 |
|||||
P275NL1 |
|||||
TStE 285 |
|||||
1.0488 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.16 | 0.40 | 0.50-1.50 | 0.025 | 0.015 | ≤ 0.30 | ≤ 0.50 |
Mo | Al | Cu | Nb | Ti | V | Ce |
≤ 0.08 | ≥0.020 | ≤ 0.30 | ≤0.05 | 0.03 | 0.05 | |
N | Co | Pb | B | Other | ||
≤ 0.020 | Nb+Ti+V≤0.05 | |||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
449 (≥) | 335 (≥) | 41 | 41 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.14 | - | |||
112 | 271 | - | 21.3 | 323 | - | ||
221 | - | 42 | 34.2 | 322 | 233 |
Heat treated : 1947°C - 1746°C
Grade | Standard | Country | Application |
---|---|---|---|
EN P275NL2 | EN | Euronorm Structural steel | |
EN P275NL2 | EN | Euronorm Structural steel |