C16 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | C16 | |||
| 15S10 | |||||
| 1.0710 | |||||
| 18S10 | |||||
| 1.0712 | |||||
| 37S10 | |||||
| 1.0713 | |||||
| 26Mn5 | |||||
| 1.0061 | |||||
| 26Mo2 | |||||
| 1.5417 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.12-0.18 | 0.40 | 0.60-0.90 | 0.045 | 0.045 | ||
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 483 (≥) | 855 (≥) | 33 | 41 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.13 | - | |||
| 694 | 435 | - | 34.3 | 213 | - | ||
| 395 | - | 41 | 13.2 | 433 | 313 | 
Heat treated : 1147°C - 1343°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| C16E | Spain structural alloy steel | ||
| EN C16E | EN | Euronorm Structural steel | |
| EN C16R | EN | Euronorm Structural steel | |
| ЖC16K-BИ | Russia | Vacuum melting of casting high temperature alloy rod | |
| ЖC16K-BИ | Russia | Standard vacuum smelting casting high temperature alloy | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com