28Cr4 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | 28Cr4 | |||
| 38Cr2 | |||||
| 1.7023 | |||||
| 1.3561 | |||||
| 44Cr2 | |||||
| 46Cr2 | |||||
| 1.7006 | |||||
| 46Cr2 | |||||
| 1.7025 | |||||
| 28Cr4 | |||||
| 1.7030 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.24-0.31 | 0.40 | 0.60-0.90 | 0.035 | 0.035 | 0.90-1.20 | |
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 227 (≥) | 671 (≥) | 33 | 11 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.31 | - | |||
| 285 | 255 | - | 42.3 | 412 | - | ||
| 476 | - | 32 | 34.2 | 443 | 322 | 
Heat treated : 1289°C - 1465°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| 28Cr4 | Spain structural alloy steel | ||
| EN 28Cr4 | EN | Euronorm Structural steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com