14NiCrMo13-4 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | 14NiCrMo13-4 | |||
| 1.6526 | |||||
| 1.6569 | |||||
| 17NiCrMoS6-4 | |||||
| 17NiCrMo6-4 | |||||
| 1.6566 | |||||
| 20NiCrMoS6-4 | |||||
| 1.6571 | |||||
| 18CrNiMo7-6 | |||||
| 17CrNiMo6 | |||||
| 1.6587 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.11-0.17 | 0.40 | 0.30-0.60 | 0.035 | 0.035 | 0.80-1.10 | 3.00-3.50 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 0.10-0.25 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 971 (≥) | 347 (≥) | 12 | 32 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 144 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.13 | - | |||
| 679 | 134 | - | 41.3 | 342 | - | ||
| 844 | - | 13 | 42.2 | 221 | 141 | 
Heat treated : 1447°C - 1876°C