Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Alloy Steel | 11564 | UNS | ||
DIN 1.7176 |
|||||
DIN 1.7218 |
|||||
DIN 1.7220 |
|||||
DIN 1.7223 |
|||||
DIN 1.7225 |
|||||
DIN 1.7228 |
|||||
DIN 1.7511 |
|||||
DIN 1.8159 |
|||||
DIN 1.0204 |
|||||
11562 |
C | Si | Mn | Ni | S | P | Cr | Mo | W | V | Ti | Cu |
0.09 - 0.16 | 0.17 - 0.37 | 0.4 - 0.7 | max 0.3 | max 0.025 | max 0.03 | 0.4 - 0.7 | 0.4 - 0.6 | max 0.2 | max 0.05 | max 0.03 | max 0.2 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
623 (≥) | 152 (≥) | 44 | 23 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.14 | - | |||
215 | 775 | - | 12.3 | 314 | - | ||
795 | - | 41 | 41.2 | 244 | 124 |
Heat treated : 1495°C - 1617°C