SUS632J2-CSP Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Stainless Steel | SUS632J2-CSP | |||
SUS436J1L |
|||||
SUS444 |
|||||
SUS444 |
|||||
SUS444 |
|||||
SUS445J1 |
|||||
SUS445J2 |
|||||
SUS301-CSP |
|||||
SUS304-CSP |
|||||
SUS420J2-CSP |
|||||
SUS631-CSP |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.09 | 1.0-2.0 | 1.0 | 0.04 | 0.03 | 13.5-15.5 | 6.5-7.55 |
Mo | Al | Cu | Nb | Ti | V | Ce |
0.4-1.0 | 0.2-0.65 | |||||
N | Co | Pb | B | Other | ||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
863 (≥) | 657 (≥) | 11 | 33 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.21 | - | |||
319 | 342 | - | 42.3 | 323 | - | ||
177 | - | 12 | 44.2 | 232 | 244 |
Heat treated : 1212°C - 1171°C