SUS347HTP Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | SUS347HTP | |||
| SUS316HTP | |||||
| SUS316LTP | |||||
| SUS316TiTP | |||||
| SUS317TP | |||||
| SUS317LTP | |||||
| SUS836LTP | |||||
| SUS890LTP | |||||
| SUS321TP | |||||
| SUS321HTP | |||||
| SUS347TP | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.04-0.1 | 1.0 | 2.0 | 0.03 | 0.03 | 17-20 | 9-13 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 8*C~1.0 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 816 (≥) | 748 (≥) | 21 | 34 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.21 | - | |||
| 355 | 714 | - | 33.3 | 411 | - | ||
| 989 | - | 33 | 34.2 | 222 | 114 | 
Heat treated : 1547°C - 1761°C