SUS317 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | SUS317 | |||
| SUS310S |
|||||
| SUS312S |
|||||
| SUS316 |
|||||
| SUS316L |
|||||
| SUS316N |
|||||
| SUS316LN |
|||||
| SUS316Ti |
|||||
| SUS316J1 |
|||||
| SUS316J1L |
|||||
| SUS316F |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.08 | 1.0 | 2.0 | 0.045 | 0.03 | 18-20 | 11-15 |
| Mo | Al | Cu | Nb | Ti | V | Ce |
| 3-4 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 341 (≥) | 159 (≥) | 31 | 33 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 44 | - | - | 0.13 | - | |||
| 526 | 444 | - | 12.3 | 232 | - | ||
| 147 | - | 22 | 12.2 | 243 | 332 |
Heat treated : 1473°C - 1572°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| SUS317LFB | JIS | Japan | austenitic special steel |
| SUS317TP | JIS | Germany | austenitic special steel |
| SUS317LTP | JIS | Japan | austenitic special steel |