X2CrNiMoN17-13-3 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | X2CrNiMoN17-13-3 | |||
| X3CrNi13-4 |
|||||
| X2CrNiN18-7 |
|||||
| X1CrNi25-21 |
|||||
| X1CrNiSi18-15-4 |
|||||
| X2CrNiN23-4 |
|||||
| X5CrNiMo17-12-2 |
|||||
| X2CrNiMo17-12-2 |
|||||
| X2CrNiMo17-13-2 |
|||||
| X2CrNiMoN17-11-2 |
|||||
| X4CrNiMo16-5-1 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| ≤0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 16.5-18.5 | 11.0-14.0 | 2.50-3.00 | N 0.12-0.22 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 724 (≥) | 124 (≥) | 13 | 32 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.34 | - | |||
| 573 | 189 | - | 12.3 | 432 | - | ||
| 741 | - | 41 | 41.2 | 221 | 332 |
Heat treated : 1899°C - 1776°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...