SUS329J4LTP Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Stainless Steel | SUS329J4LTP | |||
SUS317TP |
|||||
SUS317LTP |
|||||
SUS836LTP |
|||||
SUS890LTP |
|||||
SUS321TP |
|||||
SUS321HTP |
|||||
SUS347TP |
|||||
SUS347HTP |
|||||
SUS329J1TP |
|||||
SUS329J3LTP |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.03 | 1.0 | 1.5 | 0.04 | 0.03 | 24-26 | 5.5-7.5 |
Mo | Al | Cu | Nb | Ti | V | Ce |
2.5-3.5 | ||||||
N | Co | Pb | B | Other | ||
0.08-0.2 | ||||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
123 (≥) | 694 (≥) | 22 | 24 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.34 | - | |||
537 | 777 | - | 32.3 | 213 | - | ||
681 | - | 22 | 11.2 | 112 | 443 |
Heat treated : 1476°C - 1135°C
Grade | Standard | Country | Application |
---|---|---|---|
SUS329J4LTP | JIS | Japan | austenitic special steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com