USA AMS MAR-M 246 Cast superalloy Superalloys cast superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | MAR-M 246 Cast superalloy | AMS | USA | cast superalloy |
C | Si | Mn | S | Cr | Ni | Mo | Co | W | Al | Cu | Ti | Fe | Ta | Zr | B |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
0.13 -0.17 | ≤0.20 | ≤0.20 | ≤0.015 | 8.00 -10.00 | ≤Bal | 2.25 -2.75 | 9.00 -11.00 | 9.00 -11.00 | 5.25 -5.75 | ≤0.10 | 1.25 -1.75 | ≤1.00 | 1.25 -1.75 | 0.03 -0.08 | 0.010 -0.020 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
415 (≥) | 175 (≥) | 42 | 14 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
24 | - | - | 0.14 | - | |||
136 | 551 | - | 14.3 | 132 | - | ||
533 | - | 34 | 23.2 | 414 | 114 |
Heat treated : 1261°C - 1915°C