USA AMS AMS 5796, AMS 5759, HS 25 Superalloys Cobalt Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 52Co - 20Cr - 10Ni - 15W and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | HS 25 | AMS | USA | Cobalt Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 52Co - 20Cr - 10Ni - 15W |
C | P | Mn | S | Si | Cr | Ni | Co | Fe | W |
---|---|---|---|---|---|---|---|---|---|
0.05 -0.15 | ≤0.40 | 1.00 -2.00 | ≤0.03 | ≤0.40 | 19.00 -21.00 | 9.00 -11.00 | ≤Bal | ≤3.0 | 14.00 -16.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
281 (≥) | 113 (≥) | 44 | 34 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.41 | - | |||
466 | 493 | - | 22.3 | 241 | - | ||
964 | - | 24 | 22.2 | 112 | 231 |
Heat treated : 1249°C - 1866°C
Grade | Standard | Country | Application |
---|---|---|---|
HS-25 | |||
R30605 | |||
UNS R30605 | |||
UNS R30605 |
AMS 5796 | Cobalt Alloy, Corrosion and Heat-Resistant, Welding Wire, 52Co - 20Cr - 10Ni - 15W | AMS-5796.pdf |
AMS 5759 | Cobalt Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings, 52Co - 20Cr - 10Ni - 15W | AMS-5759.pdf |